| UNS Number | S30908 |
|---|---|
| Werkstoff Number | 1.4833 |
309S stainless steel is a highly alloyed austenitic stainless steel used for its excellent oxidation resistance, high-temperature strength and creep resistance. The lower nickel content of SS309 compared to SS310 improves resistance to hydrogen sulfide (H2S) attack at high temperatures.
309S stainless steel is an austenitic heat resisting stainless steel. 23% chromium, approx. 5% more than 304 stainless steel gives 309S stainless steel an edge over 304 stainless steel when it comes to general corrosion resistance at elevated temperatures.
309S has moderate strength and demonstrates useful performance in reducing sulphidising atmosphere


Alloy 309/309S is an austenitic chromium-nickel heat resistant stainless steel with good oxidation resistance up to 1038°C.
| Chemical Components | C | Si | Mn | P | S | Cr | Ni | Mo | N |
| Minimum | – | – | – | – | – | 22 | 12 | – | – |
| Maximum | 0.08 | 1 | 2 | 0.045 | 0.015 | 24 | 14 | – | 0.11 |
**-Slightly magnetic when cold worked.
| Diameter d mm |
Tensile Strength σb Mpa |
Yield Point σs Mpa |
Elongation δ % |
Hardness
HBW |
| Bar,Wire, Profile
160<d≤250 (+AT) |
500~750 | ≥210 | ≥30 | ≤192 |
| Bar,Wire, Profile
d≤160 (+AT) |
500~750 | ≥210 | ≥30 | ≤192 |
| Bar,Wire, Profile 63<d≤160 (+AT) | 500~750 | ≥210 | ≥30 | ≤192 |
| Bar,Wire, Profile 40<d≤63 (+AT) | 500~750 | ≥210 | ≥30 | ≤192 |
| Bar,Wire, Profile
16<d≤40 (+AT) |
500~750 | ≥210 | ≥30 | ≤192 |
| Product Form | Size Range From | Size Range To |
| Sheet & Plate | 0.30 mm | 25 mm |
| Round Bar | 4 mm | 380 mm |
| Tube | 6 mm | 260 mm |