Incoloy 825

Incoloy 825

Additional information

UNS Number

N08825

Werkstoff Number

2.4858

Description

Incoloy 825 is a nickel-iron-chromium alloy with additions of molybdenum, copper and titanium. This nickel steel alloy’s chemical composition is designed to provide exceptional resistance to many corrosive environments,that is designed to last, even under extreme operating conditions. This powerful nickel alloy is considered the forerunner of alloys containing molybdenum, the inclusion of which lends the material additional strength.In particular, in the chemical processing industry, Incoloy 825 is similar to alloy 800 but has improved resistance to aqueous corrosion.

Application

  • Sulphuric acid piping and vessels
  • Phosphoric acid evaporators
  • Pickling tank heaters, pickling tanks and equipment
  • Propellor shafts
  • Tank trucks
  • Calorifier
  • Hot vessels for food, water and seawater,
  • Ammonium sulphate vessels
  • Expansion bellows
  • Marine exhaust systems
  • Power station ash hoppers

Chemical Component

Chemical Components C Si Mn P S Cr Ni Cu Ti Al Mo Co Fe
Minimum 19.5 38 1.5 0.6 2.5 22
Maximum 0.025 0.5 1.0 0.02 0.015 23.5 46 3.0 1.2 0.2 3.5 1

 

Mechanical Properties

Tensile Strength
σb 
Mpa
Yield Point
σs 
Mpa
Elongation
δ 
%
Hardness 

HBW

≥550 ≥240 long.
≥30
≤210

Product Form

Product Form Size Range From Size Range To
Sheet & Plate 0.30 mm 25 mm
Round Bar 4 mm 380 mm
Tube 6 mm 260 mm

Request a Quote