Incoloy 901

  1. Home
  2. /
  3. Products
  4. /
  5. Incoloy
  6. /Incoloy 901

Incoloy 901

Additional information

UNS Number

N09901

Werkstoff Number

2.4662

Description

Incoloy 901 nickel-iron-chromium alloy containing titanium and aluminum for precipitation hardening and molybdenum for solid-solution strengthening. The Cr content in nickel-based alloy incoloy 901 is usually 11.0-14.0%, and the nickel content is 40-45%. The alloy has high yield strength and creep resistance at temperatures to about 1110°F (600°C). A substantial iron content enables the alloy to combine high strength with good forging characteristics.

Incoloy 901 is widely used abroad for rotating parts and fasteners on aero engines and ground gas turbines that work below 650°C, and has a long service life. It has also been used in aero engines in China, and it is a mature alloy that has passed the test of use. Alloy forging is advanced, if the process parameters are selected or operated improperly, its performance will show obvious directionality and may cause notch sensitivity, but as long as the process is strict, this phenomenon will not occur. The expansion coefficient of the alloy is close to ferritic heat-strength alloy steel, so that the two materials can be connected and there is no special requirement for the heat account.

Application

  • Heating pipes, containers, baskets and chains used in sulfuric acid pickling plants.
  • Sea water cooling heat exchanger, marine product pipeline system, acid gas environment pipeline.
  • Heat exchanger, evaporator, washing, dip tube, etc. in phosphoric acid production.
  • Air heat exchanger in petroleum refining.
  • Flame retardant alloy for high pressure oxygen application.
  • Heat exchange tubes

Chemical Component

Chemical Components C Si Mn S Cr Ni Cu Mo Ti B Al Fe
Minimum 11 40 5 2.35 0.01 Ba
Maximum 0.1 0.6 1.0 0.03 14 45 0.5 7 3.10 0.02 0.35

Mechanical Properties

Tensile Strength
σb 
ksi
Yield Point
σs 
ksi
Elongation
δ 
%
Section Shrinkage

ψ

%

≥175 ≥125 ≥15 ≥19

Product Form

Product Form Size Range From Size Range To
Sheet & Plate 0.30 mm 25 mm
Round Bar 4 mm 380 mm
Tube 6 mm 260 mm