Stainless Steel 446

  1. Home
  2. /
  3. Products
  4. /
  5. Stainless Steel
  6. /Stainless Steel 446

Stainless Steel 446

Additional information

UNS Number

S44600

Werkstoff Number

1.4749

Description

Stainless Steel 446 are known as high-alloy steels. They have excellent corrosion resistance in comparison with other steels as they contain more chromium.

Based on their crystalline structure, stainless steels are divided into three groups, namely, martensitic, austenitic and ferritic steels. A combination of martensitic and ferritic steels forms a fourth group known as precipitation-hardened steels.

The grade 446 stainless steel is a ferritic, non-heat treatable stainless steel that provides good resistance to high temperature oxidation and corrosion.

Application

Typical applications

  • X-ray tube bases
  • Boiler baffles
  • Oil burner components
  • Annealing boxes
  • Industrial mufflers
  • Kiln linings
  • Glass molds
  • Furnace parts

Chemical Component

Chemical Components C Si Mn P S Cr Ni N
Minimum 23
Maximum 0.2 1 1.5 0.04 0.03 27 0.75 0.25

Mechanical Properties

Tensile Strength

σb 

Mpa

Yield Point

σs 

Mpa

Elongation

δ 

%

Hardness 

HBW

≥515 ≥275 long.

≥20

≤217

Product Form

Product Form Size Range From Size Range To
Sheet & Plate 0.30 mm 25 mm
Round Bar 4 mm 380 mm
Tube 6 mm 260 mm

Request a Quote